Raschig GmbH, D-67061 Ludwigshafen

AMPAL MPV 2000 / Moulding compound MPV 2000 (UL gelistet / listed)
(1) Melamine-polyester, organic fibre, mineral flour (2) First Zone 60-80 °C, Düse/Nozzle 80-100 °C (3) 165-180 °C

AMPAL MPV 2500 / Moulding compound MPV 2500 (UL gelistet / listed)
(1) Melamine-polyester, organic fibre, mineral flour (2) First Zone 60-80 °C, Düse/Nozzle 80-100 °C (3) 165-180 °C

AMPAL MPV 7250 / Moulding compound MPV 7250
(1) Melamine-polyester, cellulose fibre, mineral flour (2) First Zone 60-80 °C, Düse/Nozzle 80-100 °C (3) 165-180 °C

AMPAL MPV 7270 / Moulding compound MPV 7270
(1) Melamine-polyester, cellulose fibre, mineral flour (2) First Zone 60-80 °C, Düse/Nozzle 80-100 °C (3) 165-180 °C

AMPAL MPV 7500 / Moulding compound MPV 7500 (UL gelistet / listed)
(1) Melamine-polyester, organic fibre, mineral flour (2) First Zone 60-80 °C, Düse/Nozzle 80-100 °C (3) 165-180 °C

MELOPAS MF 150 / Moulding compound MF 150, Typisierte Formmasse nach ISO 14528 / Standardized moulding compound to ISO 14528
(1) Melamine-formaldehyde, wood flour (2) First Zone 70-90 °C, Düse/Nozzle 90-100 °C (3) 165-180 °C

MELOPAS MF 152 / Moulding compound MF 152, typisierte Formmasse nach ISO 14528 / Standardized moulding compound to ISO 14528
(1) Melamine-formaldehyde, cellulose fibre (2) First Zone 70-90 °C, Düse/Nozzle 90-100 °C (3) 165-180 °C

MELOPAS MF 152.7 / Moulding compound MF 152.7, typisierte Formmasse nach ISO 14528 / Standardized moulding compound to ISO 14528
(1) Melamine-formaldehyde, cellulose fibre (2) First Zone 70-90 °C, Düse/Nozzle 90-100 °C (3) 165-180 °C

MELOPAS MF 180 / Moulding compound MF 180, typisierte Formmasse nach ISO 14529 / Standardized moulding compound to ISO 14529 (UL gelisted / listed)
(1) Melamine-phenolic, wood flour (2) First Zone 70-90 °C, Düse/Nozzle 90-100 °C (3) 165-180 °C

MELOPAS MF 181 / Moulding compound MF 181, typisierte Formmasse nach ISO 14529 / Standardized moulding compound to ISO 14529 (UL gelisted / listed)
(1) Melamine-phenolic, cellulose fibre (2) First Zone 70-90 °C, Düse/Nozzle 90-100 °C (3) 165-180 °C